Aluminum Silicate, Extender Slurries (Formulation #21-10006) Patcham LTD Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing f...展开 Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. 收起
Calcium Carbonate, Extender Slurries (Formulation #21-10006) Patcham LTD Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing f...展开 Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm/ gauge 7+ NS. 收起
Interior/Exterior Gloss Paint (Formulation #21-10005) Patcham LTD Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...展开 Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind at 4 ms-1 until desired Hegman gauge is achieved- 7+ NS/ <10 μm. 收起
Interior/Exterior Matt Paint (Formulation #21-10005) Patcham LTD Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...展开 Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind at 4 ms-1 until desired Hegman gauge is achieved. 5+ NS/ min. of 20 μm. 收起
Interior/Exterior Semi Glossy Paint Waterborne Coatings (Formulation #21-10005) Patcham LTD Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...展开 Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind at 4 ms-1 until desired Hegman gauge is achieved. -7 NS/ min. of 15 μm. 收起
Talc, Extender Slurries (Formulation #21-10006) Patcham LTD Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...展开 Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. 收起
Zinc Oxide, Extender Slurries (Formulation #21-10006) Patcham LTD Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...展开 Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. 收起