Polycarbonate (PC): HiFill FR®
Product | Availability | Product Description |
---|---|---|
HiFill FR® J-50/20/FR | Africa & Middle East |
Molding Parameters:
4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing.
The dry temperature at 16 hours is 180°F.
For 2-zone machines, the rear temperature is 550-590°F, and the front temperature is 540-560°F.
|
HiFill FR® J-50/30/FR | Africa & Middle East |
Molding Parameters:
4 hours recommended for high tensile strength and smooth surface finish, or for vacuum metalizing.
The dry temperature at 16 hours is 180°F.
For 2-zone machines, the rear temperature is 550-590°F, and the front temperature is 540-560°F.
|
HiFill FR® PC 1001 FR-NR | North America | |
HiFill FR® PC 1003 FR-NR UV | North America | |
HiFill FR® PC 1003 UV | North America | |
HiFill FR® PC FR 06 NAT | North America | |
HiFill FR® PC FR IM | North America | |
HiFill FR® PC GF10 FR BK | North America | |
HiFill FR® PC IM FR | North America | |
HiFill FR® PC MCF/GB 1525 BK001 | North America | |
HiFill FR® PC/ABS FR NH | North America |