Patcham is a world-wide supplier of an expansive range of paint driers and coatings additives. They also have a considerable amount of knowledge in the formulation of plant tinters and colorants. Their Pat-Add range of products include slip and leveling agents, wetting and dispersing agents and defoamers. Their Patcom range of driers are either lead free or cobalt free systems used to speed the rate of drying in Air Drying Systems. All products are low or no VOC as well as being APEO free.
9 Resultados
Aluminum Silicate, Extender Slurries (Formulation #21-10006) Patcham USA Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing f...Vea Mas Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. Vea Menos
Calcium Carbonate, Extender Slurries (Formulation #21-10006) Patcham USA Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing f...Vea Mas Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm/ gauge 7+ NS. Vea Menos
Interior/Exterior Gloss Paint (Formulation #21-10005) Patcham USA Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...Vea Mas Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind at 4 ms-1 until desired Hegman gauge is achieved- 7+ NS/ <10 μm. Vea Menos
Interior/Exterior Matt Paint (Formulation #21-10005) Patcham USA Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...Vea Mas Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind at 4 ms-1 until desired Hegman gauge is achieved. 5+ NS/ min. of 20 μm. Vea Menos
Interior/Exterior Semi Glossy Paint Waterborne Coatings (Formulation #21-10005) Patcham USA Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...Vea Mas Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind at 4 ms-1 until desired Hegman gauge is achieved. -7 NS/ min. of 15 μm. Vea Menos
Solventborne 2K PU White Topcoat (Formulation #21-20001) Patcham USA This solventborne 2K PU white topcoat features Pat-Add DA 1801. It is suitable for general industrial coatings, wood coatings, and auto refinish coatings.
Talc, Extender Slurries (Formulation #21-10006) Patcham USA Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...Vea Mas Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. Vea Menos
Waterborne Epoxy Primer (Formulation #21- 10001) Patcham USA This waterborne epoxy primer features Pat-Add DA 817. It is suitable for general industrial coatings.
Zinc Oxide, Extender Slurries (Formulation #21-10006) Patcham USA Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...Vea Mas Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. Vea Menos