Nubicem 101 Pigment Concentrate For Silicate And Lime Paints, 50% (Formulation #W4516) Ferro Pigments Pigment concentrate of ultramarine blue for applications to high pH.
Nubicoat HWR Pigment Concentrate for Silicate and Lime Paints, 50% (Formulation #W2947) Ferro Pigments Pigment concentrate of ultramarine blue for applications to high pH.
RA 40 Pigment Concentrate for Silicate and Lime Paints, 50% (Formulation #W2947) Ferro Pigments Pigment concentrate of ultramarine blue for applications to high pH.
V8 Pigment Concentrate for Silicate and Lime Paints, 50% (Formulation #W2947) Ferro Pigments Pigment concentrate of ultramarine blue for applications to high pH.
Water-borne Vinyl Acrylic Dispersion Primer (Formulation #3.2) GRACE Water-borne Vinyl Acrylic Dispersion Primer (Formulation #3.2) is a guideline formulation offered to show reduced blistering and wet dispersion loss at the scribe compared to a control bank. Haloflex 202 is a water thinnable vinyl-acrylic dispersion with an acidic pH. The addition of Alcophor 827 is beneficial in two respects: the pH is stabilised at 6.5 which would otherwise be buffered by SHIELDEX® anti-corrosive pigments, and it also improves the corrosion resistanceafter hot salt spray and humidity exposure. The addition level of SHIELDEX® anti-corrosive pigments should not exceed 3 wt.-% to ensure that the pH ...view more Water-borne Vinyl Acrylic Dispersion Primer (Formulation #3.2) is a guideline formulation offered to show reduced blistering and wet dispersion loss at the scribe compared to a control bank. Haloflex 202 is a water thinnable vinyl-acrylic dispersion with an acidic pH. The addition of Alcophor 827 is beneficial in two respects: the pH is stabilised at 6.5 which would otherwise be buffered by SHIELDEX® anti-corrosive pigments, and it also improves the corrosion resistanceafter hot salt spray and humidity exposure. The addition level of SHIELDEX® anti-corrosive pigments should not exceed 3 wt.-% to ensure that the pH of the final formulation does not exceed 7. view less
Nubicem B-101 Concentrate at 50% for Silicate and Lime Paints Ferro Pigments This formulation is a pigment concentrate of Ultramarine Blue with high color stability at high pH and Ca2+. It is recommended for decorative and architectural paints, white correction, and DIY.
Interior/Exterior Gloss Paint (Formulation #21-10005) Patcham USA Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...view more Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind at 4 ms-1 until desired Hegman gauge is achieved- 7+ NS/ <10 μm. view less
Aluminum Silicate, Extender Slurries (Formulation #21-10006) Patcham USA Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing f...view more Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. view less
Calcium Carbonate, Extender Slurries (Formulation #21-10006) Patcham USA Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing f...view more Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm/ gauge 7+ NS. view less
Interior/Exterior Matt Paint (Formulation #21-10005) Patcham USA Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...view more Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind at 4 ms-1 until desired Hegman gauge is achieved. 5+ NS/ min. of 20 μm. view less
Interior/Exterior Semi Glossy Paint Waterborne Coatings (Formulation #21-10005) Patcham USA Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...view more Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind at 4 ms-1 until desired Hegman gauge is achieved. -7 NS/ min. of 15 μm. view less
Talc, Extender Slurries (Formulation #21-10006) Patcham USA Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...view more Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. view less
Zinc Oxide, Extender Slurries (Formulation #21-10006) Patcham USA Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...view more Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. view less